PECVD aligned CNT array sealed with spin-on glass |
Sealing thinckness:1-3 microns.
|
 |
 |
A PECVD aligned array sealed with spin-on glass. Click image above for large view.
|
Exposed nanotube cross sections from a spin-on-glass-sealed array after mechanical polish. Click image above for large view.
|
|
 ,
|